【summary】
In general, amorphous plastics such as PC, PMMA and ABS, etc., the mother without adding color is transparent, and there is no specific requirement for its thickness. But the thickness of welding semi-crystalline plastics is generally not more than 2 mm , because the mother without adding color is milky white or milky yellow. When containing glass fiber plastics, the thickness should be as small as possible on the basis of ensuring the mechanical properties of the parts. 1. It is recommended to use PBT material with a thickness of less than 1.5mm. 2. Using nylon material, the thickness is recommended to be less than 2mm. 3. Using POM material, the thickness is recommended to be less than 3mm.
General principle, amorphous plastics such as PC, PMMA and ABS, etc., the mother without adding color is transparent, and there is no specific requirement for its thickness. But the thickness of welding semi-crystalline plastics generally does not exceed 2mm, because the mother without adding color is milky white or milky yellow. When containing glass fiber plastic, the thickness should be as small as possible on the basis of ensuring the mechanical properties of the parts.
1. It is recommended to use PBT material with a thickness of less than 1.5mm.
2. Using nylon material, the thickness is recommended to be less than 2mm.
3. Using POM material, the thickness is recommended to be less than 3mm.
| Free solutions/free proofing 13710252340
Previous: What is a typical weld design?